Spring Bar Steel, Hot Rolled (56Si7)
The advantage of our hot rolled spring steel is that there are high thicknesses possible. As the tensile strength of the bars is 900-1100 N/mm² it may be necessary to do a heat treatment after fabrication of your parts an before using them.
The bars can be cut in length according to your wishes.
| Material | Material Number |
|---|---|
| 56Si7 | 1.5026 |
| Material Standard |
DIN EN 10089 |
| Dimension standard |
DIN EN 10092-1 |
| Replaced dimension standard |
DIN 4620 |
| Supplied Conditions | Standard: + AR (as rolled), on request: +S (treated for shearability), +A (soft annealed), +AC (annealed to achieve spherical carbides) |
| Products |
Flat |
| Dimensions | Thickness: 4-25 mm |
| Edges | EN 10092-1-F-A (semicircular) | EN 10092-1-F-B (semi-rounded side) | EN 10092-1-F-C (rounded edges) |
| Tensile strength (Rm) | Approx. 900-1100 N/mm² in +AR condition, can be subsequently hardened to higher strengths |
| Surface | hot rolled, untreated |
| Information |
|
| Heat Treatment |
|
Chemical analysis (in %) according to EN 10089, Table 3
| Material Code | 56Si7 |
| C | 0,52 - 0,60 |
| Si | 1,60 - 2,00 |
| Mn | 0,60 - 0,90 |
| P | ≤ 0,025 |
| S | ≤ 0,025 |
| Cu+Sn | Cu+10Sn± 0,60 |